The 5Ni@NC-400H catalyst with Ni2N6 sites showed 99.5% of FECO for CO2RR to CO at −0.77 V and FECO retained >99% from −0.37 to −1.17 V vs. RHE in flow cell. The CO2 activation at Ni2N6 sites occurs via bridging absorption of reaction intermediates.